Abstract

Pin holes as a surface defect, and blow holes as an inner defect, occur in billet / bloom / beam blank casting, particularly for Si-Mn killed steel cast with metering nozzle and oil lubrication. If they are present in abundance or have a large size, they may originate defects in the rolled products. Their characteristics, factors behind their formation, as well as usual processing conditions that promote their occurrence are discussed. Finally, the evolution of these defects during reheating and rolling is analyzed, with industrial examples.
Citation

APA: Jorge Madias  (2017)  Billet Defects: Pin-hole And Blow-hole Formation, Prevention And Evolution

MLA: Jorge Madias Billet Defects: Pin-hole And Blow-hole Formation, Prevention And Evolution. Associacao Brasileira de Metalurgia, Materiais e Mineracao, 2017.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account