Blast Furnace Test Of Pelletech Cold Bond Pellets

Society for Mining, Metallurgy & Exploration
M. Adnan Goksel
Organization:
Society for Mining, Metallurgy & Exploration
Pages:
11
File Size:
879 KB
Publication Date:
Jan 1, 1979

Abstract

A blast furnace test of approximately 5,000 tons of PelleTech Corporation (PTC) cold bond pellets was successfully run at Kaiser Steel Corporation (Kaiser) Steel Manufacturing Division at Fontana, California. The pellets were produced from mill scale, BOF dust and blast furnace flue dust. A 15 day base period, during which time the metallic burden was 2/3 heat indurated pellets and 1/3 sinter, preceeded the test. During the test period the metallic bur- den was 10% cold bond pellets, 56.7% heat indurated pellets and 33.3% sinter. A 15 day post test base period followed during which the PTC pellets were replaced by conventional pellets. The pellets were produced in the 3.C Semi-works Facility located on Kaiser property. The facility incorporates the Michigan Technological University Hydro-Thermal Agglomerating Process.
Citation

APA: M. Adnan Goksel  (1979)  Blast Furnace Test Of Pelletech Cold Bond Pellets

MLA: M. Adnan Goksel Blast Furnace Test Of Pelletech Cold Bond Pellets. Society for Mining, Metallurgy & Exploration, 1979.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account