Development of Ni-Co-Base Superalloys for Turbine Disk Applications
    
    - Organization:
 - Canadian Institute of Mining, Metallurgy and Petroleum
 - Pages:
 - 8
 - File Size:
 - 1101 KB
 - Publication Date:
 - Jan 1, 2006
 
Abstract
"A new kind of cast & wrought (C&W) Ni-Co base superalloys named as ""TMW alloys"" are developed recently for compressor or turbine disks of gas turbine engines in High Temperature Materials 21 Project at National Institute for Materials Science (NIMS) in Japan. These Ni-Co base superalloys combine the characters of two kinds of y- y' two-phase alloys (Ni-base and Co-18at%Ti alloys) and have higher tensile strength and creep resistance than C&W UNDIMET 720Li superalloy."
Citation
APA: (2006) Development of Ni-Co-Base Superalloys for Turbine Disk Applications
MLA: Development of Ni-Co-Base Superalloys for Turbine Disk Applications. Canadian Institute of Mining, Metallurgy and Petroleum, 2006.