Abstract

Energy required for roasting and smelting of a nickeliferous laterite ore by the rotary kiln - electric furnace process is investigated. From this work it comes that thermal energy is about 65% of the total energy needed and the rest is electrical. Also, 61.3% of thermal energy input in the roasting step (of all combustibles fed into the rotary kilns) is used for pre - heating, 11.6% for pre - reduction and the rest (27.1%) corresponds to the energy of the remaining carbon in the rotary kiln products (i.e., calcine, dust and coatings). Carbon entering the system is used as follows: 57.9% for combustion, 37.1% for reduction and the rest (5.0%) remains unburnt. Exploitation of energy from gases of both furnaces, as well as the higher possible reduction degree, the optimum temperature of the calcine and also elimination of the excess air in the rotary kilns, improve significantly energy balance and economics of the process.
Citation

APA: Emmanuel N. Zevgolis  (2006)  Energy Requirements In Nickeliferous Laterite Treatment

MLA: Emmanuel N. Zevgolis Energy Requirements In Nickeliferous Laterite Treatment. The Minerals, Metals and Materials Society, 2006.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account