Abstract

Considerable mechanical property decline is always observed at the Heat Affected Zone (HAZ) of AA 5083, This occurred as a result of the thermal effect on the hardened material, It is highly beneficial to have a prospective metallurgical procedure to overcome this decline of properties. Therefore, experiments were set to evaluate the effectiveness of a quick post weld heat treatment process with the AA 5083, Optimum results were obtained at 473K and with approximately 600 seconds time, The interplay between the time, temperature and mechanical properties are possible to explain by the Lifshitz-Slyozov-Wagner (LSW) theory and by considering the composition of the material.
Citation

APA: W. Mirihange  (2005)  Enhancement of mechanical properties in heat affected zone of AA 5083 weld joints: Potential and interpretation

MLA: W. Mirihange Enhancement of mechanical properties in heat affected zone of AA 5083 weld joints: Potential and interpretation. Canadian Institute of Mining, Metallurgy and Petroleum, 2005.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account