Abstract

Fe-Ni alloys can be used as raw material in making stainless steel. Laterite nickel ore is one of mineral resources for producing nickel alloys. In this work, the laterite ore after dehydration at 800 °C and the anthracite as reducing agent were mixed for pre-reduction at 900 °C, and then reduced to form Fe-Ni alloys at 1550-1620 °C through carbon-thermal reduction process. A high Ni-content alloy component in the metallurgical mixture can be formed through pre-reduction. Better separation of the resulting metals from the slag is found with lower Ni-content alloys produced or higher temperatures during reduction. An effective processing of Fe-Ni alloys needs further understanding of the process fundamentals and optimizing of the process parameters.
Citation

APA: Jilai Xue  (2010)  Fe-Ni Alloys Formation in Carbonthermal Reduction Process using Laterite Nickel Ore

MLA: Jilai Xue Fe-Ni Alloys Formation in Carbonthermal Reduction Process using Laterite Nickel Ore. The Minerals, Metals and Materials Society, 2010.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account