Fine Grinding o f Ore by Tube.Mills. and Cyaniding at El Oro. Mexico

The American Institute of Mining, Metallurgical, and Petroleum Engineers
G. Caetani
Organization:
The American Institute of Mining, Metallurgical, and Petroleum Engineers
Pages:
53
File Size:
1978 KB
Publication Date:
Jan 1, 1906

Abstract

I. INTRODUCTION. WE owe to the courtesy of Mr. R. M. Raymond, Manager of the El Oro Mining & Railway Co., Ltd., the permission of publishing in this paper the results of a series of experiments and tests made in view of determining the economical limit to which the fine grinding of the ore by tube-mills could be carried on. For the sake of clearness, the following definitions are given of certain terms used in this paper, as well as of the units and screens in the experiments. Slime : In a general way " slime" is that mill-product, of which from 90 to 95 per cent, will pass a 200-mesh screen (0.067 mm. aperture), and which is treated as one class of material in the El Oro cyanide-plants. As a screen-product, slime constitutes all material that *ill pass a 200-mesh, screen. In sizing, the following products are distinguished:- Coarse Sand : That material remaining on a 100-mesh (0.111 mm. aperture) screen. Fine Sand : That passing through. 100-mesh and remaining on a 200-mesh (0.067 mm. aperture) screen. Slime: That passing through 200-mesh. Fines, which pass through 200-mesh and settle in 30 seconds, and silt, which does not settle in 1 minute. Sand-index : The number proportional to its total fineness considered from the economical point of view, as explained on page 93. Absolute extraction : The percentage of values actually brought into solution. Actual extraction: The percentage of values actually brought to the ziuc-boxes. Units : Dollars, U. S. Currency; pounds; and short tons (2,000 lb.). Gold is valued at $20.67, and silver at $0.50 per ounce. Screens : In the sizing-tests the screens used were:¬ Mesh (per 1 in.), . 24 30 40 60 80 100 150 200 250 Aperture (mm.), . 0.740 0.515 0.424 0.250 0.159 0.111 0.090 0.067 0.058 Strengths of solution : Strengths are expressed in the percent- . age of KCN contained, though the sodium cyanide, which is
Citation

APA: G. Caetani  (1906)  Fine Grinding o f Ore by Tube.Mills. and Cyaniding at El Oro. Mexico

MLA: G. Caetani Fine Grinding o f Ore by Tube.Mills. and Cyaniding at El Oro. Mexico. The American Institute of Mining, Metallurgical, and Petroleum Engineers, 1906.