Improving Rechargeable Hydrogen Storage Capacity Of BCC Alloy By Eliminating Internal Defects

The Minerals, Metals and Materials Society
Toshiki Kabutomori
Organization:
The Minerals, Metals and Materials Society
Pages:
8
File Size:
1334 KB
Publication Date:
Jan 1, 2006

Abstract

In fuel cell powered automobiles, hydrogen is required to be stored in materials that have a hydrogen storage density of over 4 mass%; further, these materials should be capable of supplying hydrogen by using the waste heat from a fuel cell, which is at a temperature of 373 K, in order to match the mileage of gasoline-powered vehicles. A Ti-Cr-V alloy, which exhibits a BCC structure and forms a solid solution, is a promising candidate for onboard hydrogen storage materials. Although it has a large hydrogen storage capacity of over 3.9 mass%, the rechargeable hydrogen capacity is limited to approximately 2.6 mass%. In this study, the effects of fine pulverization of the alloy on PCT (hydrogen pressure-composition-isotherm) characteristics were investigated in order to improve the rechargeable hydrogen storage capacity of the alloy. From the PCT measurements of the finely pulverized samples of the alloy, a plateau in the absorption curve was observed to begin at a hydrogen concentration of 0.5 mass%; further, a rechargeable hydrogen storage capacity of 3.3 mass% was obtained. This was greater than that obtained from the sample that was not finely pulverized, i.e., 2.5 mass%. However, the plateau width in the desorption curve was 2.5 mass%, which was the same as that observed for the sample that was not finely pulverized. The increase in the rechargeable hydrogen capacity during absorption is attributed to the precipitation of the -hydride phase (MH~2) directly from the metal phase (phase). The precipitation of the phase (MH~0.5), which should be formed in low hydrogen concentrations, is suppressed as a result of a possible reduction in the internal defects such as dislocations, vacancies, and grain boundaries by fine pulverization and annealing of the alloy.
Citation

APA: Toshiki Kabutomori  (2006)  Improving Rechargeable Hydrogen Storage Capacity Of BCC Alloy By Eliminating Internal Defects

MLA: Toshiki Kabutomori Improving Rechargeable Hydrogen Storage Capacity Of BCC Alloy By Eliminating Internal Defects. The Minerals, Metals and Materials Society, 2006.