Influence of TCP Phase on Enduring Property of Single Crystal Nickle-Based Superalloys
- Organization:
- The Minerals, Metals and Materials Society
- Pages:
- 8
- File Size:
- 6154 KB
- Publication Date:
- Jan 1, 2010
Abstract
By means of the measurement of the enduring property and microstructure observation, an investigation has been made into the influences of the element Re and TCP phase on the enduring property of the single crystal nickel base superalloys. Results show that the needle-like TCP phase is precipitated along the <110> orientation on {111} planes in Re-containing/free superalloys during the long term aging, the TCP phase is identified as µ phase, and the precipitated µ phase in 4.5%Re alloy is gradually spheroidized during aging. Thereinto, the needle-like µ phase may obviously decrease the enduring lifetimes of the alloys due to the consumption of the refractory elements and the effect of the stress concentration. But the stress concentration is not easily generated in the regions near the spherical-like µ phase, which is a main reason of reducing the enduring lifetime of 4.5%Re alloy to a small extent.
Citation
APA: (2010) Influence of TCP Phase on Enduring Property of Single Crystal Nickle-Based Superalloys
MLA: Influence of TCP Phase on Enduring Property of Single Crystal Nickle-Based Superalloys. The Minerals, Metals and Materials Society, 2010.