Abstract
Typically, rougher molybdenite flotation and recovery from bulk copper/ molybdenum concentrates involves the use of alkalisulfides, Nokes reagents, cyanides, oxidants, and/or thermal treatment for the depression of copper sulfide minerals. The bulk copper/molybdenum feed generally varies from 0.2% Mo to 1.0% Mo, and with traditional reagents the single-stage rougher flotation recovery of molybdenite varies between 40 and 90% at a concentrate grade of 5 to 10% Mo. With ozone conditioning for copper depression, however, improved separations appear to be possible, as demonstrated by tests with Cu/Me concentrates from both the Phelps Dodge Morenci Operations and the Kennecott Copperton Operations. Single-stage rougher flotation after ozone conditioning can provide a molybdenum concentrate at a recovery of more than 90% and a rougher concentrate grade higher than 20% Mo in some cases. Subsequent cleaner flotation with additional ozone conditioning results in relatively copper-free molybdenum concentrates containing as much as 52% Mo. Preliminary analysis indicates that, with a multistage ozone conditioning/flotation strategy, the process is technically and economically viable and should be suitable for industrial application.
Citation
APA:
(1990) Molybdenite Flotation From Copper/Molybdenum Concentrates By Ozone Conditioning (db26685c-10b3-4bd2-b48c-69e9624125ef)MLA: Molybdenite Flotation From Copper/Molybdenum Concentrates By Ozone Conditioning (db26685c-10b3-4bd2-b48c-69e9624125ef). Society for Mining, Metallurgy & Exploration, 1990.