The procedure to arrive at an energy efficient autogenous grinding plant is carried out in the following steps: First Step - Determine power requirements to grind a particular ore. This work carried out on small samples ground in a 450 mm diameter Aerofall Hill and the results are checked against a standard Bond Index test. Second Step - A bulk sample from the ore zone is ground in a 1.8 m diameter pilot mill. This work is carried on until the power objectives as indicated from the first step have been realized. Third Step - Correlate the pilot mill data, with the data from the numerous samples ground in the small 450 mm mill and arrive at design criteria for the commercial plant. Ensure commercial mill design will be suitable to obtain similar results as those obtained in the pilot mill.
Citation

APA: A. R. MacPherson  (1981)  Power Efficient Autogenous Grinding Plants

MLA: A. R. MacPherson Power Efficient Autogenous Grinding Plants. Society for Mining, Metallurgy & Exploration, 1981.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account