Abstract

As part of a comprehensive investigation of tie mechanism of desufurization of iron and steel by slags, the Blast Furnace Studies Section, Metallurgical Division, Bureau of Mines, in cooperation with the Institute of Technology-, University of Minnesota, has made a study of the forms in which sulfur occurs in blast-furnace slag. This report presents data on the three sulfides most important in iron smelting, namely, ferrous sulfide, manganous sulfide, and calcium sulfide. The tendency of these sulfides to form colloids in the molten slag was determined by an examination of quenched samples with an ultramicroscope. Vogt5/ conducted experiments on sulfide silicate melts and examined synthetic blast-furnace slags in a partly crystallized condition. His conclusions were that FeS, CaS, and bins, or isomorphous compounds, such as (FexCay)S and (MnxCy)S, were precipitated Prom the melt, depending on the composition of the slag. In all specimens sulfides were visible and were spherical.
Citation

APA: Allan E. Martin  (1941)  RI 3552 Form Of Sulfur Occurrence In Blast-Furnace Slag - Introduction (8eea1b30-bdf1-466d-bc2b-bfc531c84416)

MLA: Allan E. Martin RI 3552 Form Of Sulfur Occurrence In Blast-Furnace Slag - Introduction (8eea1b30-bdf1-466d-bc2b-bfc531c84416). The National Institute for Occupational Safety and Health (NIOSH), 1941.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account