RI 8020 Rock Fragmentation by High-Frequency Fatigue

The National Institute for Occupational Safety and Health (NIOSH)
Patrick J. Cain
Organization:
The National Institute for Occupational Safety and Health (NIOSH)
Pages:
24
File Size:
6181 KB
Publication Date:
Jan 1, 1975

Abstract

The fatigue-failure characteristics under high-frequency (10 KHz) cyclic loading were determined for a marble, granite, and quartzite. The rock speci-mens were cyclicly loaded (using a high-power piezoelectric sonic transducer) at a constant strain amplitude generated by forming a longitudinal standing stress (strain) wave in the cylindrical test specimen. The number of load cycles required to fail each rock type at a given strain amplitude was deter-mined. The fatigue fractures were tensile in nature and the fracture load amplitudes were as low as 30 pct of the static tensile strength. Also the internal heating of the rock caused by the material damping (internal friction) was measured. The damping and internal heat generation in the specimens was analyzed to show that nearly all of the power input can be accounted for as a change in enthalpy in the specimen. Using these results the thermal strain in the rock was calculated to evaluate its contribution to fatigue failure. The thermal strain was found to range up to 30 pct of the dynamic strain amplitude depending on the load amplitude and the number of load cycles. The specific energy required for failure was determined and possible applications of the high-frequency fatigue fragmentation process are discussed.
Citation

APA: Patrick J. Cain  (1975)  RI 8020 Rock Fragmentation by High-Frequency Fatigue

MLA: Patrick J. Cain RI 8020 Rock Fragmentation by High-Frequency Fatigue. The National Institute for Occupational Safety and Health (NIOSH), 1975.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account