San Francisco Paper - Zinc-Dust Precipitation Tests (with Discussion)

- Organization:
- The American Institute of Mining, Metallurgical, and Petroleum Engineers
- Pages:
- 9
- File Size:
- 407 KB
- Publication Date:
- Jan 1, 1916
Abstract
The use of zinc dust for precipitating the pecious metals from cyanide solutions is well established now in many places, and has many advantages over the shavings method of precipitation. Although much work has been done o,n methods of testing zinc dust, as yet. no absolutely positive test has been devised to determine the value of the material. Certain facts are known, but often it happens that results on a working scale are not as expected from the laboratory tests. The purpose of this paper is to record some obscrvations made while testing a large variety of zinc-dust samples in the laboratory. W. J. Sharwoodl has described standard analytical methods, which have been followed, with the changes noted. The regular determinations include zinc oxide, by solution in ammonia and ammonium chloride, lead, and precipitating efficiency. In some cases cadmium was determined by a method similar to that described by J E Clennell.2 I will discuss the precipitating-efficiency test in detail. The procedure is as follows: "A solution of potassium silver cyanide is prepared by dissolving 10 grams of silver cyanide (AgCN) and 5 grams of 99 %' potassium cyanide in a little water and diluting up to 1000 cc. It is then adjusted by addition of a little more XCN or AgCN until the solution indicates from 0.12% to 0.15% free KCN by titration with standard silver nitrate. The titration is best made by using a 10-cc. or 20-cc. sample, adding 1 CC. of 2 % potassium iodide, and a slight excess of ammonia, as the end point is then sharper. Or 15 grams of pure crystallized XAg(CN)2 may be dissolved in a liter of water and 1.5 grams XCN added. " Weigh out 0.5 gram zinc dust into a 300-cc. beaker. Add a few cubic centimeters of watcr and stir until zinc is well mixed, then pour in 250 cc. of the prepared solution, stirring vigorously. See that all lumps are broken up, and continue stirring for fully five minutes. Stir occasionally (at least every 10 minutes) until the end of two hours from the addition of the solution. Then filter upon an 11-cm. filter, wash precipitate thoroughly, sprinkle with test lead, wrap it carefully in the paper, place in a scarifier with about 20 grams test lead, burn paper cautiously in muffle, scorify five minutes, cupel at low temperature and weigh silver. Milligrams silver obtained from 0.5 gram zinc X 0.0606 = percentage precipitating efflciency."³
Citation
APA:
(1916) San Francisco Paper - Zinc-Dust Precipitation Tests (with Discussion)MLA: San Francisco Paper - Zinc-Dust Precipitation Tests (with Discussion). The American Institute of Mining, Metallurgical, and Petroleum Engineers, 1916.