The Application Of Trend Surface Analysis To The White Pine Copper Deposit ? Introduction

Society for Mining, Metallurgy & Exploration
S. C. Nordeng
Organization:
Society for Mining, Metallurgy & Exploration
Pages:
11
File Size:
1531 KB
Publication Date:
Jan 1, 1964

Abstract

The program described in this paper is primarily a test of the possible utility of multiple regression in ore search, It was carried out as a cooperative project between White Pine Copper Company, the Institute of Mineral Research and the Department of Geological Engineering of the Michigan College of Mining and Technology. The authors wish to thank Dr. Cleaves Byers, Associate Professor of Mathematics, MCM&T, and Mr. Robert DeBaubien, Graduate Student in Mathematics, MCM&T, for their work in programming the project for the computer,
Citation

APA: S. C. Nordeng  (1964)  The Application Of Trend Surface Analysis To The White Pine Copper Deposit ? Introduction

MLA: S. C. Nordeng The Application Of Trend Surface Analysis To The White Pine Copper Deposit ? Introduction. Society for Mining, Metallurgy & Exploration, 1964.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account