Abstract

The Plant. The annual production of the Pyhasalmi mine is 900 000 tons of copper- zinc-pyrite ore containing approximately 0.7 % Cu, 2.5 % Zn and 30 % S. During 1976...1981 altered surface ore, 850 000 tons in all, was also treated at the concentrator. The surface ore was crushed and ground in a separate plant and was then fed into the copper or zinc flotation or was flotated in its own circuit, depending on the degree of alteration and the content of copper and zinc in the ore. The surface ore was exhausted in October 1981. Flotation comprises three consecutive flotation circuits; copper, zinc and pyrite circuit. The zinc circuit includes an open circuit roughing and scavenging. The scavenger concentrate and cleaner tailing are pumped to the middlings flotation. Rougher concentrates of the open circuit and the middlings flotation are pumped to cleaning which includes four stages. Figure 1 describes the flowsheet of the zinc circuit.
Citation

APA: Jorma Miettunen  (1982)  The Control Strategy Of Zinc Flotation At The Pyhäsalmi Mine ? Introduction

MLA: Jorma Miettunen The Control Strategy Of Zinc Flotation At The Pyhäsalmi Mine ? Introduction. Society for Mining, Metallurgy & Exploration, 1982.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account