Abstract

"Compared with conventional roasting and magnetic separation processes, higher reduction temperatures and stronger reducing atmospheres are used in reduction technologies to reduce iron oxides to metallic iron, which is often liberated during reduction and amenable to magnetic separation. Reduction and magnetic separation of an Australian refractory iron ore was therefore studied as a function of reduction temperature, time and coal addition. It was found that during reduction, the particle size of the reduced iron increased with reduction temperature and time. Subsequent magnetic separation tests were further conducted on the reduction products. A reduced iron powder with a Fe grade of 85.67 per cent was obtained at a Fe recovery of 87.82 per cent under optimum reduction conditions where a metallisation rate of 85.82 per cent was achieved. The mechanism involved in reduction is discussed based on XRD and SEM examinations.CITATION:Han, Y X, Liu, J, Li, Y J and Zhang, S M, 2013. Upgrading an Australian iron ore by reduction and efficient magnetic separation, in Proceedings Iron Ore 2013, pp 397-402 (The Australasian Institute of Mining and Metallurgy: Melbourne)."
Citation

APA: Y X. Han J Liu Y J. Li S M. Zhang  (2013)  Upgrading an Australian Iron Ore by Reduction and Efficient Magnetic Separation

MLA: Y X. Han J Liu Y J. Li S M. Zhang Upgrading an Australian Iron Ore by Reduction and Efficient Magnetic Separation. The Australasian Institute of Mining and Metallurgy, 2013.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account