Determination Of Crystallite Size And Surface Roughness Of Copper Deposits For Electrowinning In The Presence Of An Organic AdditiveBy Cesimiro Fabian
The crystallite size of copper electrodeposits was determined by X-Ray powder diffraction analysis using a General Area Detector Diffraction Solution (GADDS) diffractometer. Crystallite size was calc
Jan 1, 2003
-
Flotation Of Colloidal Lead Carbonate Using Series Of Spargered Flotation CellsBy F. J. Tavera
The colloid flotation of lead carbonate precipitates in aqueous media is studied at a pH of 7. The flotation system consisted of five spargered flotation cells in a serial array. The flotation system
Jan 1, 2006
-
Mechanism Of Electrolysis Of Rare Earth Chlorides In Molten Alkali Chloride Baths (Invited)By Tsutomu Yamamura
The electrolytic reduction mechanism of rare-earth chlorides such as LaCl3, CeCl3, NdCl3, ` SmCl3 and DyCl3 in alkali chloride baths has been investigated in NaCl, KCI and eutectic LiCI- KCI by means
Jan 1, 2003
-
Rejected Sands from Smelting Metallurgical Process Used in Structural CeramicsBy Fabio J. Esper, Guillermo R. Martín-Cortés, Francisco R. Valenzuela-Díaz, Cassio P. Carvalho, Giorgio Grotti, Reginaldo B. Santos
"Rejected sands from smelting metallurgical process because contain lead and others heavy metals are a problem to dispose as waste in all the countries. A procedure that is being proposed for it is to
Jan 1, 2008
-
Assessment of Ladle Slag as Binder Alternative for Cold Bonded BriquettesBy Daniel Adolfsson, Ryan Robinson, Fenwei Su, Jelena Blagojevic
"Cold bonded briquetting of steel plant by-products has proven to be a viable recycling alternative concerning technology, economy and environment in both the traditional blast furnace route and the d
Jan 1, 2008
-
Sidewall Design to Improve Lining Life in a Platinum Smelting FurnaceBy I. Mc Dougall
"The matte/slag tidal zone in a platinum smelting furnace is subject to severe process conditions which can often lead to premature failure of the lining. The MgO-FeO-Si02 slag is aggressive to refrac
Jan 1, 2012
-
Reduction of Carbon Dioxide to Formate in an Electrochemical Membrane Reactor in KHCO3 Buffer SolutionsBy G. Gomathi, K. Asokan, K. Subramanian
An electrochemical reactor with anode and cathode chambers separated by a composite perfluoro polymer cation exchange membrane was designed, fabricated and used for the reduction of dissolved carbon d
Jan 1, 2008
-
Upgrade of Mixed C & DW Recycled Aggregates Quality by Automatic SortingBy Anette Mueller, Thomas Schnellert, Sérgio C. Angulo
"The use of automatically sorting technique, to separate gypsum components from recycled material of processed construction and demolition waste (C&DW), is motivated by environmental and economical as
Jan 1, 2008
-
Precious Metal Recovery with Electronically Conducting PolymersBy A. C. Cascalheira, L. M. Abrantes, M. Savic
This paper reports our results on the application of a novel process for the spontaneous and sustained reduction and recovery of elemental silver and gold on an electroactive polymer surface. This wor
Jan 1, 2000
-
Structurally Sound Metal Parts by Selective Laser SinteringBy Mukesh K. Agarwala
Alloy composite parts were made from powders by Selective Laser Sintering (SLS). SLS is a rapid prototyping process that uses data from CADICAMICAE systems to guide a laser beam and rapidly form 3-D p
Jan 1, 1994
-
Activity Measurement Of The Constituents In Molten Sn-Ag-In And Sn-Zn-Mg Ternary Lead Free Solder Alloys By Mass SpectrometryBy Takahiro Miki
Soldering material widely used is Sn-Pb alloy, which have low melting point and excellent electrical, strength properties and wettability. However, Pb is one of the toxic elements, which is undesirabl
Jan 1, 2003
-
Activity Measurement Of The Constituents In Molten Sn-Ag-In And Sn-Zn-Mg . Ternary Lead Free Solder Alloys By Mass SpectrometryBy Takahiro Miki
Soldering material widely used is Sn-Pb alloy, which have low melting point and excellent electrical, strength properties and wettability. However, Pb is one of the toxic elements, which is undesirabl
Jan 1, 2003
-
Kinetics of the Transpassive Oxidation of Coal PyriteBy Xirneng Zhu
The electrochemical behavior of Pittsburgh and Illinois coal pyrite in basic and neutral borate/sulfate solutions was investigated. In the transpassive region, aggressive oxidation of pyrite occurred.
Jan 1, 1994
-
Effect Of Atmosphere Composition On Sintering Of BronzeBy Garg. D.
Premixed bronze powders are widely used to produce a wide variety of P/M components including bearings and bushings by the powder metal industry. The physical and mechanical properties of sintered bro
Jan 1, 1996
-
Microstructural Characterization of Aluminum Metal Matrix Composite Prepared by In-Situ MethodBy Dumitru Mitrica, Vasile Soare, Elvira Alexandrescu, Mihai Ghita, Marian Burada, Petru Moldovan, Raluca Maria Florea
"Aluminum metal matrix composite Al-Si /SiCp was prepared by reactive gas injection and subsequent remelting. The influence of the remelting process on the microstructure and physicalmechanical proper
Jan 1, 2014
-
Fate Of Sulphide Sulphur In Bacterial Oxidation Of Sulphide MineralsBy H. Kandemir
An experimental study of the bacterial oxidation of naturally occurring high-purity sulphide minerals (FeS2, Fe1-xS, Cu5FeS4, ZnS) is presented using a mesophilic strain of T. ferrooxidans. As well as
Jan 1, 1985
-
Characterization of Copper Vermiculite Antibacterial NanomaterialBy Bowen Li
Copper vermiculite is a special nanomaterial with excellent antibacterial and antifungal performance. By means of ion exchange, copper vermiculite containing up to 5.8wt% copper was prepared. The chem
Jan 1, 2003
-
Extraction of Zinc From Chloride Solution with DBBPBy Hsing Kuang Lin
Extraction of zinc from chloride solution with dibutyl butylphosphonate (DBBP) in Escaid 110 has been investigated. The distribution coefficient of zinc was found to be independent of equilibrium pH.
Jan 1, 1990
-
The Removal of Nickel from Leachate of Galvanic Sludge with Titanium DioxideBy Ozgul Dere Ozdemir, Muge Sari Yilmaz, Sabriye Piskin, Deren Sibel Kasap
"Galvanic sludge is generated at the end of the waste water treatment process of metal plating system. The waste sludge is one of the main hazardous solid wastes produced by metallurgical industries.
Jan 1, 2011
-
Vapor Pressure Measurements For The FeCl2-ZnCl2 System By The Transpiration Method (1590c387-bb76-43a1-a5ba-66c736f9b1b5)By Sang Han Son
The vapor pressures of FeCL2 and ZnCL2 in the FeCL2?ZnCL2 system were measured by the transpiration method at 873K and 9I7K, The vapor pressure data were interpreted to indicate the formation of compl