Search Documents
Search Again
Search Again
Refine Search
Refine Search
-
Physical Modeling of Three-Phase Mixing in a Counter-Current Reaction Launder (CCRL) Process for Metal RefiningBy Lloyd R. Nelson
Experimental results of three-phase mixing in a physical model of a CCRL for metals refining are presented. The system was operated above a critical lower liquid height-to- width ratio (H,/W) of unity
Jan 1, 1995
-
The Steps Required to Meet Production Targets at PT TNCO, Indonesia: A New Innovative Business StrategyBy Chris Doyle
From 1997-2000. PT INCO undertook the Fourth Line Expansion Project (FLEX) to increase annual production rates from 90-100 to 150 Mlbs Ni/year (68,000 MT Ni/yr). In 2003, PT INCO nickel production und
Jan 1, 2004
-
Upgrade of Mixed C & DW Recycled Aggregates Quality by Automatic SortingBy Anette Mueller, Thomas Schnellert, Sérgio C. Angulo
"The use of automatically sorting technique, to separate gypsum components from recycled material of processed construction and demolition waste (C&DW), is motivated by environmental and economical as
Jan 1, 2008
-
Synthesis of Ultrafine Intermetallic Particles by the Vapor-Phase Coreduction of Metal Chlorides with HydrogenBy H. Y. Sohn, S. PalDey
"Fine particles of nickel aluminides and Ni4Mo were synthesized by reducing mixtures of, respectively, A1Cl3 + NiC12 and NiC12 + MoC12 vapors with hydrogen. Though thermodynamically favorable, the cor
Jan 1, 1998
-
Characterization of Fly Ash from a Municipal Solid Waste IncineratorBy John W. Graydon
Incineration is an attractive alternative to the disposal of MSW in landfill sites. However, the process of incineration generates fly ash which contains significant levels of leachable heavy metals -
Jan 1, 1992
-
Mixture Design Applied to the Electrochemical Reduction of CaW04 to WBy Metehan Erdogan, Orhan Gökçe Göksu, Ishak Karakaya
"An experiment (mixture) design was created to optimize the process parameters of the electrochemical reduction of CaW04 to W in molten CaCl2-NaCl eutectic mixture. Temperature, applied voltage and th
Jan 1, 2012
-
Determination Of Crystallite Size And Surface Roughness Of Copper Deposits For Electrowinning In The Presence Of An Organic AdditiveBy Cesimiro Fabian
The crystallite size of copper electrodeposits was determined by X-Ray powder diffraction analysis using a General Area Detector Diffraction Solution (GADDS) diffractometer. Crystallite size was calc
Jan 1, 2003
-
Climate Change and Metal & Mining Sector: An Overview of Trends, Project Potential and its AbatementBy P. K. N. Raghavan
This paper identifies potential technologies for Carbon dioxide abatement from the mining and metal industry with special reference to the Aluminium industry. Mine reclamation could contribute to this
Jan 1, 2011
-
Rejected Sands from Smelting Metallurgical Process Used in Structural CeramicsBy Fabio J. Esper, Guillermo R. Martín-Cortés, Francisco R. Valenzuela-Díaz, Cassio P. Carvalho, Giorgio Grotti, Reginaldo B. Santos
"Rejected sands from smelting metallurgical process because contain lead and others heavy metals are a problem to dispose as waste in all the countries. A procedure that is being proposed for it is to
Jan 1, 2008
-
The Role Of Lead Smelting At Korea ZincBy Chang-Young Choi
Korea Zinc commenced zinc production in 1978 with a capacity of 50,000 tpa. Since then, continuous investments have been made and resulted in Korea Zinc now being the biggest zinc and lead producer in
Jan 1, 2003
-
Relationship between the Surface Tensions and the Compositions of Copper and Nickel MattesBy Zhang Hengzhong
Based on thermodynamics of surfaces and a proposed two-dimensional state equation for surfaces, the relationship between the surface tension (Y) of a solution and the activity (a1) of its component (i
Jan 1, 1993
-
Kinetics Of Biological Ferrous Iron OxidationBy Paul L. Wichlacz
A mathematical model of growth and ferrous iron oxidation for attached bacteria was applied to rotating biological contactor (RBC) units treating acidic mine drainage. The model describes attached bac
Jan 1, 1985
-
Expansion of the Rio Tinto Patino Tankhouse at HuelvoBy C. Palacios
The Plant, which was started up in April 1970, was originally designed for a capacity of 40.000 ton of cathodes per annum, using 12 sections, containing 408 cells. Since then the addition of another 8
Jan 1, 1976
-
Sidewall Design to Improve Lining Life in a Platinum Smelting FurnaceBy I. Mc Dougall
"The matte/slag tidal zone in a platinum smelting furnace is subject to severe process conditions which can often lead to premature failure of the lining. The MgO-FeO-Si02 slag is aggressive to refrac
Jan 1, 2012
-
Hybrid Porous Metal of Nano-Micro Double Size and Regular-Random BimodalBy Xingming Zhang, Huawei Zhang, Yanxiang Li
"A hybrid porous metal with nano-micro double scale pore size and regular-random bimodal porous structure has been fabricated by unidirectional solidification of a lotus-type alloy followed by dealloy
Jan 1, 2014
-
Recovery of Copper from a-Etchant SolutionBy C. W. Won
a-etchant solution is the waste material obtained during the etching by ammoniacal solution of printed circuits for PCs. This material contains a substantial amount of copper (13-14%) but is usually d
Jan 1, 1993
-
Kinetics of Non-Isothermal Precipitate Process of Perovskite Phase in CaO-TiO2-SiO2-AI2O3-MgO SystemBy Li Yuhai
Kinetics of non-isothermal precipitate process and crystal growth of perovskite (CaO ? Ti02) phase in CaO-TiOz-Si02-AlP3-MgO system were studied. The experimental results show that the relative volume
Jan 1, 2000
-
Synthesis Of Ultra-Fine LiFePO4/C And Its Electrochemical PerformanceBy Hong Liang-shi
Olivine lithium iron phosphate (LiFePO4) is considered as one of the most promising materials for lithium-ion secondary batteries because of its high theoretical capacity, low cost, good safety, benig
Jan 1, 2006
-
Dissolution And Precipitation Processes In The Secondary Separation Of Rare EarthsBy K. Osseo-Asare
Aqueous stability diagrams (25°C) are presented for the systems M-H2O and M-Oxalate-H2O where M=Sm, Nd, Co, and Fe. With the aid of these diagrams (i.e., Eh-pH and log[Metal]- log[Oxalate]), the solut
Jan 1, 1997
-
Characterization of Nanocrystalline Silver Fabricated by Warm-Vacuum-Compaction MethodBy Qionghua Zhou, Wei Liu
"Nanocrystalline silver bulk material with average grain size of 20.3 nm was prepared by warmvacuum- compaction method. The as-prepared nanocrystalline silver was characterized by X-ray diffraction (X
Jan 1, 2011